Ceramic Inclusion Stains
Sino's inclusion stains solve the problem that cadmium red can't resist high temperature.
They are very stable in the glaze which contains lead, calcium, or boron. If the content of the alkali metal in the giaze is too high, it will damage the included layer of the stains, and also degrade the color. So the grinding of the stain can't last long time.
The temperature range covers: 800°C-1280°C
Code No. |
Name |
Composition |
Max Firing Temp |
Firing condition |
Color |
SIS300B |
Pale yellow |
Cd-Si-Zr-S |
1280 |
Oxide |
|
SIS300 |
Yellow |
Cd-Si-Zr-S |
1280 |
Oxide |
|
SIS300A |
Dark yellow |
Cd-Si-Zr-S |
1280 |
Oxide |
|
SIS301C |
Orange yellow |
Cd-Si-Zr-Se-S |
1280 |
Oxide |
|
SIS301 |
Orange yellow |
Cd-Si-Zr-Se-S |
1280 |
Oxide |
|
SIS301A |
Orange yellow |
Cd-Si-Zr-Se-S |
1280 |
Oxide |
|
SIS301B |
Orange red |
Cd-Si-Zr-Se-S |
1280 |
Oxide |
|
SIS306 |
Red |
Cd-Si-Zr-Se-S |
1280 |
Oxide |
|
SIS306A |
Red |
Cd-Si-Zr-Se-S |
1280 |
Oxide |
|
SIS306B |
Red |
Cd-Si-Zr-Se-S |
1280 |
Oxide |
|
SIS306C |
Dark Red |
Cd-Si-Zr-Se-S |
1280 |
Oxide |
|
SIS309 |
Dark Red |
Cd-Si-Zr-Se-S |
1280 |
Oxide |
|
|